Search Casting Studies



There are 86 studies matching your search criteria.

Aquahalo cover ring

View

The use of zinc and die-casting technology in sanitary engineering consistently yields top-tier technical results. This application area places particular demands on surface design, dimensional stability, and tolerance accuracy. The AQUAHALO cover ring, part of a...

Automatic force wedge

View

The automatic force wedge shown is part of the additional locking devices of the mechanical-automatic door lock “Roto Safe A | Tandeo”. With this door lock, front doors can be locked automatically without using a key. In conjunction with an additional drive unit, the...
ima01

Automotive Shift Level

View

This shift lever connects the shifter and the gear in ZF automotive gearboxes. This part was originally cast in aluminum but required tapping and other secondary operations in order to meet the close tolerances. Thanks to close collaboration with the customer, the...
ima10

Bayonet XT-A

View

The 3-piece bayonet XT-A is assembled into a circular piece and provided with a cover plate. The part is designed so that it connects with an inlay heatsink, necessary due to the heat generated by the installed LED (60-80°C). The casting challenge is to achieve a...
Bearing_attatchment

Bearing Attachment

View

ln this example, a ball bearing housing which is die cast in alloy Z410 (equivalent to BS 1004B) is attached to a thin continuously electrogalvanized steel sheet pressing. Studs – integral rivets – are cast into the housing. After the steel pressing is located, the...
blackpl2_photo2_caseID68

Blackplate support pad for pin printer

View

Modern printers require a pin support which must be cast pore free, non-deformable, and of precise dimensions. Because of the large numbers of units produced, the life of the die is a determining factor. From the client’s point of view, the sound dampening qualities...

Busbar for electric fan

View

  As an individual part, the award-winning casting is a very filigree, long and sensitive component. Four individual and very thin conductor strands with dimensions in the millimeter range have to be produced by casting with a cross-section of perhaps just one...
capstan2_photo2_caseID70

Capstan Retainer

View

Precision and strength are important design considerations for the minicartridge tape drive, and the capstan retainer is a good example. This part is actually two separate components cast together–a Torx head screw with an integral retainer sleeve. To produce the...

Case for Wendt & Kühnangel figure

View

The award-winning cast part “suitcase” is based on the original of a suitcase and represents a decorative part in the series of collectible dolls, made of wood. While suitcases were made of leather many decades ago, there was a separate edge protection...
ima04

Central Console

View

Utilizing zinc alloys to create this part allowed for outstanding control of each step and parameter involved in the full process, from design to final part to achieve, to achieve the perfect design. With die casting, the same surface quality and appearance could be...
ima08

Central Support Unit

View

This part is a central support unit for mounting all optical, electrical, and mechanical components for the imaging plate technology in use in dentistry. In medical technology, die cast zinc has been used for many years; however, overall, this area of ​​application is...
channel2_photo2_caseID71

Channel and T-shape

View

This two-piece holder was developed for a precision scientific instrument. Both castings have detailed features requiring tolerances of +/-0.00025 in. Extrusion could not be used because it could not hold the tolerances, while CNC and wire EDM were not cost effective....
chassis2_photo2_caseID72

Chassis, Shield and Synthesizer Housing

View

The Ericsson GE Mobile Communications’ M-PA personal radio incorporates three Zamak 3 die castings: the chassis or circuit board frame, the chassis shield, and the synthesizer housing. These castings combine to provide strength and rigidity demanded for...
checkva2_photo2_caseID73

Check Valve

View

Previously, the check valve was assembled from machined aluminium bar stock and brass pipe fittings. A net shape die casting was designed by consolidating the six-piece assembly into a single, net shape component. All holes and seven thread sets, including a male...

Closure ring overhead shower RAINFINITY

View

In the field of sanitary technology, extremely high demands are placed on the surface appearance, resistance and dimensional stability of the assemblies. A high standard of haptics conveys a high-quality feeling. With the casing of the Rainfinity overhead shower, the...
compute2_photo2_caseID77

Computer Rear Cover

View

Micro-informatics are already an integral part of business and professional life. The will soon be present everywhere, including the home. What role do zinc alloys play? This back cover for a microcomputer illustrates how zinc die castings can simplify design and...
ima15

Connector for Radio AM/FM Signal

View

The part has the following attributes: One of this part’s highlights is its functionality—it allows one single part in Zamak for electrical connection (interface) and mechanical (coding + retention). It also has a connector function, which allows for the transmission...
connect2_photo2_caseID79

Connector Housing – Berg Electronics MICROPAX ™ connectors

View

MICROPAX connectors have very demanding specifications which are met by zinc die casting, including: Complex design requirements to accommodate a variety of connectors, ranging from 40 to 200 connecting pins; flatness across the mounting plane within +/- 0.005 in, and...
control2_photo2_caseID80

Control Boxes

View

The control boxes for Minn Kota electric motors went through several design phases before settling on zinc die casting as the material/process of choice. The boxes were originally sand cast aluminium and later die cast aluminium. Short tool life prompted engineers to...
cableconnect2_photo2_caseID128

Copper Cable Connectors

View

Zinc die casting was chosen to produce this new generation of cable connectors. Critical standards that were met include wall strength to assure durability and to withstand bulk processing and proper matching of draft allowances on the internal surfaces for smooth...

Corner Stake – Security Door

View

The zinc pressure die cast corner stake, fastened with pop rivets, fits tightly into the Galvabond roll form section of the door. It has to compete with plastic molded, aluminium extruded, and aluminium pressed parts’ this is because of the many properties of the zinc...

Cover for a high-quality sanitary shower system

View

  Today, bathrooms are no longer just places to shower, wash your hands or freshen up. Today, bathrooms are high-quality experience spaces and oases of well-being. Value is placed on good products with perfect surfaces. Function and control of cold and warm water...
ima01

Cover Plate e-drive

View

This part is used in a drive system as a special shield to guarantee good air ventilation in addition to perfect cooling of the system. Reasons for choosing zinc alloy include the complex tool design; requirement to cast the part to size; ability to forego using...
ima13

Dental – Occlusal Bite Holder Block

View

The medical sector is a highly demanding, niche market. The main benefit of using zinc die casting for this product is the outstanding surface quality achieved.
differe2_photo2_caseID112

Different Parts

View

Cost savings were the initial reason for converting a number of steel stampings into this single zinc die casting. The surface flatness and dimensional precision between features such as fixing studs was greatly improved, this permitted more reliable assembly of...
doorbra2_photo2_caseID166

Door Brake

View

Automatic closing mechanisms for swing doors have to be adjustable and brake the movement of the door. The mechanism must be strong, resistant, reliable, and compact enough to be housed in a casing. Pressure injected zinc alloy casings offer undeniable advantages,...

Door closure system INSTINCT by MACO

View

Smart Home is becoming an increasingly important part of our daily lives. A large number of household appliances, from dishwashers to water purifiers, can now be operated via smartphones. Why not also window and door fittings? With the innovative, fully electronic...
fitting2_photo2_caseID168

DragonFly (TM) camp stove – Mountain Safety Research

View

The original fuel fitting design was an assembly of three screw-machined components–a brass orifice, an aluminum stop block and lock mount, and a stainless steel hose barb. By redesigning the assembly as a one-piece zinc die casting, a 56 percent cost reduction was...
drivede2_photo2_caseID132

Drive Beck

View

The drive deck for Cherokee’s 5-1/4 in. WORM optical drive utilizes a ZA-12 graphite permanent mold casting. From the start, graphite permanent mold was the process of choice because of its economical tooling cost, good dimensional control, and low-volume economies....
driving2_photo2_caseID170

Driving Gears

View

This is an excellent alternative to engineering plastics, aluminium or milled – sintered steel for the realization of driving gears for toothed belts (electronics) or pinion engagement (building, mechanical, precision hardware). Off-tool net shape thin wall zinc die...
ima14

Electronic Connector

View

The key benefits to this product’s design was a close cooperation between die caster and customer through a clipping system. It utilizes modern assembling technology, and because it does not involve a screw, creep is not a risk.
ima11

Electronics Housing

View

SINAMICS Control Unit CU305  This casting is a housing for the most demanding industrial electronics. To avoid short circuits, it needs to be free of residual particles. To save costs for post-processing and cleaning steps, a net-shape mold concept was developed....

Escutcheon for overhead shower for Grohe Rainshower series

View

The award-winning component is a large-scale application of die-cast zinc as a shower head. The large surface area of ​​the cover rosette component of an overhead shower for the GROHE Rainshower series in connection with a galvanic surface treatment places special...

Front part of fountain pen

View

Handle recesses and push-button covers for electronic front door locks and windows increasingly have to fulfill more than just mechanical functions; they are now being equipped with electronics to enable fingerprint access, integrate LED lighting, and control electric...
gearrac2_photo2_caseID115

Gear Rack and Housing

View

One of the first opportunities to test ACuZinc 5 was in Delphi Interior and Lighting System’s newly-designed heliscrew horizontal actuator for power seats. The die castings replace a powder-metal gear rack and plastic gear housing design. Seat adjustment is comparable...
gridmod2_photo2_caseID116

Grid Module

View

Mosaic mimic panels form a display system that provides an overall picture of complex operations and gives technicians the ability to monitor and control events. The system’s main advantage is its modular design, providing flexibility for easy modification and...
handlea2_photo2_caseID83

Handle and Backplate

View

Pictured is one model of a range of decorative door handles. Zinc is used for the design because of its ability to easily take a plated finish and because it can be cast to accurate dimensions.
handlel2_photo2_caseID84

Handle and Lock Assembly

View

In both residential and commercial construction projects, architects are frequently asked to design large windows and sliding glass doors. Sliding doors must be easy and comfortable to operate from either inside or outside, and it must be possible to lock them. Zinc...
handlef2_photo2_caseID85

Handle for Electrical Cabinet

View

This zinc alloy part is designed to raise the global quality perception of the final product. The dimensional precision of the process for the fine fitting of different sub assemblies and the long life of the mold and tooling for large production series led the choice...
ima07

High Tension Cage

View

This part is a device component warranting the operators security during intervention on high-tension lines. The reasons behind choosing zinc alloy include the product’s complex tool design, the combination of thin wall casting and rigidity, and the dimensional...
housinf2_photo2_caseID89

Housing & Frame

View

The elements of this equipment (TYCAS) were created to detect the positions of approaching aircraft according to new security norms of the IATA. The process proved to be more economical compared to traditional machining despite limited series and to pressure die cast...
housinb2_photo2_caseID90

Housing and Base Plate

View

Originally, the housing and base plate frame were sand cast aluminium and finish machined. Machining and assembly time took 3.5 hours per unit. During a redesign, the company set about to reduce costs without sacrificing quality or performance. This led to graphite...
ima09

Housing for electro-tool

View

The drive head of this tool, made out of 2 parts, is cast in ZP5.  This casing contains the gear that translates rotating and oscillating movements at very high rpm and frequencies. The part needed to comply with low tolerances for shape and position in both...
ima05

Housing for HSD Connector

View

This HSD connector (HSD = high speed data) is a part of the control units in upper segment cars. The 4-pin connector assures large volume of data transfer as compared to the standard connector with only 1 pin. The required tolerances for this miniature part are...
ima03

Housing for KitchenAid Coffee Machine

View

The 9,5 kg zamak housing of this designer coffee machine is made from 8 zinc pressure die cast parts with weights between 2.2 kg and 75 g. The parts are powder coated. To avoid any bubbles during thermal curing of the paint, the parts are vacuum cast to avoid gas...

Housing for low voltage angle gear drive

View

This casting is a segment of a multi-piece gearbox for 24/48 volt engines. The cost pressure in the market segment prompted the designers to rethink. A cost-effective production method for manufacturing the individual components that does not require any further...

Housing MX bottom shell R2S3

View

With this modular concept, various pluggable, cast housing components can be installed in the system as required. The concept implements a new, complex and resource-saving control cabinet technology. The combination of system function modules and a housing base...
lawnedg2_photo2_caseID96

Lawn Edge Trimmer

View

The innovative Qualcast Lawn Edge Trimmer, the design of which is patented, is entirely based on zinc castings, which are used for both drive train and housings. The trimmer is attached to the standard Concorde mower by replacing the existing belt drive cover with a...
ima08

LEO Easy Opener

View

This design opener can open all kind of bottles without any damage and with very little effort. With its innovative patented mechanism, this tool won the Bundespreis 2016 award in Germany. ZP5 was chosen over other materials for its excellent surface finish, strength,...
micropr2_photo2_caseID106

Microprocessor Protection Housing

View

This part can be created in large production volumes. Assembly is uncomplicated even with complex shapes, competing with pressed steel sheet. Zinc castings’ superior thermal conductivity permits faster and greater heat dissipation provided by thinner radiating fins,...
lasermt2_photo2_caseID107

Microscan Systems – VS 310 Scanner

View

Designers of an ultra-compact scanner needed to reduce the internal envelope. The optics bracket was one component that was reduced in size but increased in functionality. The goal was to design a single mounting bracket that would accommodate a laser module, a...
microwa2_photo2_caseID177

Microwave Guides (5 configurations)

View

Wave guides are built to exacting specifications in dimensional accuracy, straightness, and flatness. Hot chamber die casting enables critical cavity sections to be cast with little or no draft; very difficult in aluminium cold chamber die casting. Flatness tolerance...
gearbox2_photo2_caseID129

Miter Gear Box – Hunter Douglas Venetian Blind

View

A four-piece miter gear assembly utilized zinc die casting for strength and precision. Both pinion gear shafts and housing halves are die cast net-shape, achieving full functionality without a cost penalty compared to alternative designs (thermoplastic housing/gears...

Mobile Radio Antenna

View

Zinc die casting was chosen to reduce cost of an antenna base for mobile radio equipment, which was originally a brass screw-machined part. Powder metallurgy was evaluated, but it couldn’t achieve the required undercuts without machining. Zamak 2 alloy was specified...
modular2_photo2_caseID179

Modular Base Plate

View

This part is a modular base plate working in a pneumatic environment. Its function is to transport air between an air distributor and a jack. Modular base plates are made of pressure die cast Zamak 5 (ZA4UIG). The excellent fluidity of zinc alloys provides a surface...
motorch2_photo2_caseID118

Motor Chassis

View

This chassis for a motor drive unit for an automatic opening roller door was made from several pressed metal parts prior to being designed as a zinc die casting. Die casting in zinc alloy 3 provided numerous benefits: 1.) Additional features such as pockets, the...

Motorcycle indicator housing BMW R18

View

For many, the BMW R18 brings back memories of the old days – cruising alone on winding roads, a comfortable ride and good road holding. The vehicle has to have a certain solid and sonorous appearance. With the R18 model, BMW is addressing the buyers of a Harley...

MX housing bottom shell

View

A product extension has been developed for an innovative modular control cabinet solution from Beckhoff, based on the plug-and-play principle. A cast base shell has been designed for a new module that can be plugged into the modular system. Since control cabinets and...
paperfe2_photo2_caseID109

Paper Feeding Guide for Thermic Printer

View

The anti-magnetic character of the zinc alloys combined with the economic advantages of the production process win over the press formed steel sheet and aluminium profiles.

Planter Handler

View

The planter handle is used to adjust spring force to a pair of closing wheels. It is important for the handle to be durable, easily accessible, and very comfortable to grip. To accent product appearance, designers chose a die cast over a welded fabrication. Die cast...
quickclamp2_photo2_caseID182

Quickclamp Air Prep System – IMI Norgren

View

A newly designed air preparation system utilizes zinc die casting for the major components of the Quickclamp(TM) assembly (as well as the bodies, bowls, and accessory parts of the filters, regulators and lubricators). Die cast zinc provides greater strength than...
reducti2_photo2_caseID145

Reduction Gear

View

The seats in luxury cars are moved forwards and backwards by motorized reduction gears which must be solid, reliable, accurate, and mechanically strong. Zinc alloys satisfy these requirements and offer the added benefit of noise reduction due to their density.
reducto2_photo2_caseID147

Reductor

View

Zinc’s excellent bearing properties at high loads and low speeds permitted it to be used for this part without the use of pressed-in bronze bearings, reducing cost. The required dimensional precision and high required strengths also made zinc die casting the preferred...

Remote car release key, design elements

View

People carry this cast part with them in many variations: a design element of the car key. The demand for a high-quality look, an appealing, cool feel and the requirements for a robust, largely scratch-resistant surface led to the decision to use zinc as a material....
ima04

Remote Control

View

This high-end remote control’s design has tactile control without any knobs. The zamak surface was cast to a thickness of 0.6mm with less than 0.05mm tolerance on thickness. Piezo elements translate the bending of the surface into electric signals. For casting this...

Shielded connector for electrical engineering

View

Plug connections in electrical engineering are highly complex components that have to be delicate yet stable due to the space available. Added to this is the shielding function of different conductors in the housing. The award-winning shield housing is a true...

Shift paddles on a Porsche steering wheel

View

A zinc die-casting application in the absolute premium range: This award-winning cast part is tangible on the steering wheel of a Porsche sports car and makes acceleration an experience. The paddles are attached to both sides of the back of the steering wheel and are...
ima02

Steering Column Housing

View

Key benefits include: Design and use of a complex tool to avoid multiple secondary operation.  Excellent gating control to achieve mechanical tolerances.
ima06

Subframe and Carriage

View

The three parts of this design form a subassembly that measures the thickness of ophthalmic lenses before edging. The frame ensures the palpate lever guidance in the ophthalmic glass machine tool. Then, the glass is machined with the contour note during the palpate...
ima09

Support Unit for Drive

View

This product is a segment drive for imaging plate technology used in dentistry. A complex, modern, and advanced die casting enables precise and optimum shape design that is consistent with the mechanical properties of the die cast zinc alloy. In medical technology,...

The key safe

View

The SUDHAUS key safe is a secure storage place for keys and other valuables. The dimensions were chosen so that bunches of keys and credit card formats can be stored. Areas of application include contactless key handover for holiday homes, rental car collection/return...
ima05

Thermostate Valve Housing

View

Special features of this die cast product include precise dimensions that ensure a perfect fit around the circumference of the housing, making it water-resistant so that the internal components are protected. The tool design allows for uniform filling and casting with...
topandb2_photo2_caseID155

Top and bottom sensor plate – dollar bill changer

View

A dollar bill changer incorporated top and bottom sensor plates fabricated from welded stamped components. The weldments could not hold tolerances greater than +/- 0.020 in. In an effort to resolve dimensional instability and fit problems, the manufacturer, working...
tracing2_photo2_caseID125

Tracing Machine

View

Océ Graphics – one of the world’s leading manufacturers of tracing machines –  uses zinc alloy die castings in each of the seven machines in its range. Zinc alloy castings form part of the structure of the machines, through the two side plates and two grips in the...
ima11

Traffic Light Housing

View

Together, these two parts form a protective casing for the internal components of traffic lights. The material properties provide protection against vandalism and have much longer lifetimes than polymer materials. Due to thinner sections, they are also lighter than...
tunerho2_photo2_caseID157

Tuner Housing

View

Two M4 threads were needed on this zinc die casting in Z410 alloy (equivalent to BS 1004B). Because the holes were at 90° and in different planes, the threading could not be carried out in a single operation. By comparison with two separate threading operations, it...
visecom2_photo2_caseID160

Vise Components

View

Eight separate ZA-12 alloy castings are utilized in the TUCKER woodworking vise. Castings form the pivot block, front jaw, rear jaw, quick-release nut, yoke, stanchion, mounting plate, and keeper plate. Based on the shapes needed to form the vise, casting easily...
wavegui2_photo2_caseID190

Waveguide Horn

View

The Whistler Spectrum 3SE waveguide horn is a complex Zamak 3 die casting providing detail, net shape, and thin wall construction. The current horn replaces three separate pieces utilized in earlier models. One component now performs four distinct functions: a horn...
wirejoi2_photo2_caseID191

Wire Jointing Device

View

Estate Wire Ltd. established a massive potential market for a simple but effective wire jointing device. A specialized design consultancy service – Cheshire Engineering Ltd. – was commissioned to investigate the possibilities. After rejecting a number of alternatives,...

X-ray dental technology housing

View

  The award-winning casting is characterized by a completely different zinc die-cast property than strength, filigree and thin walls. Due to its use as a component of an X-ray device, thick-walledness, tightness and also precision are in demand. In addition, the...
xraytan2_photo2_caseID161 (1)

X-ray tank+lock+guide Tube Assembly

View

The X-ray tank + lock + guide assembly consists of a very high frequency generator for dental radiology. The parts in this assembly are made of pressure die cast Zamak 5 (ZA4IUG), an alloy which offers the following functions for this application: mechanical strength,...
platen3_photo3_caseID163

Z Series Printers – Zebra Technologies

View

The platen housing design incorporates three previous parts. In order to function properly, the material must be rigid and strong. The housing is cast with four elongated slots, four deep slots, and seven cored holes, maximizing the need for structural support. In...