Casting Study: Different Parts

Major Selection Criteria: Complex Shape, Dimensional Precision, Integration of Multiple Functions
Alloy: Zamak 3 (ZL3, ZL0400, ZnAI4, alloy 3)
Application Field: Industrial
Application Size: 320 x 220 x (2-3) mm / 12.60 x 8.66 x (0.08-0.12) inches - largest
Surface Finish: As-Cast
Casting Technique: Pressure Die Casting
Source: A.M.I. Fonderie

differe2_photo2_caseID112Cost savings were the initial reason for converting a number of steel stampings into this single zinc die casting. The surface flatness and dimensional precision between features such as fixing studs was greatly improved, this permitted more reliable assembly of rotating shafts and bushings. The surface finish of the part was also greatly improved.