Casting Study: Steering Column Housing

Major Selection Criteria: Complex Shape, Dimensional Precision, Integration of Multiple Functions, Mechanical Properties, Net Shape
Alloy: Zamak 5 (ZL5, ZL0410, ZnAI4Cu1, alloy 5)
Application Field: Automotive
Application Size: 100-250 g
Surface Finish: As-Cast
Casting Technique: Pressure Die Casting
Source: DYNACAST Osterreich GmbH

ima02Key benefits include:

  • Design and use of a complex tool to avoid multiple secondary operation. 
  • Excellent gating control to achieve mechanical tolerances.