Search Casting Studies



There are 26 studies matching your search criteria.

Bearing_attatchment

Bearing Attachment

View

ln this example, a ball bearing housing which is die cast in alloy Z410 (equivalent to BS 1004B) is attached to a thin continuously electrogalvanized steel sheet pressing. Studs – integral rivets – are cast into the housing. After the steel pressing is located, the...

Busbar for electric fan

View

  As an individual part, the award-winning casting is a very filigree, long and sensitive component. Four individual and very thin conductor strands with dimensions in the millimeter range have to be produced by casting with a cross-section of perhaps just one...
chequeg2_photo2_caseID74

Cheque Guide

View

This single zinc die casting replaced an assembly of stainless steel components. By use of a single casting, rigidity was greatly improved and dimensional precision between critical dimensions was made more reliable. Zinc die casting permitted the required dimensional...
differe2_photo2_caseID112

Different Parts

View

Cost savings were the initial reason for converting a number of steel stampings into this single zinc die casting. The surface flatness and dimensional precision between features such as fixing studs was greatly improved, this permitted more reliable assembly of...
valvespace2_photo2_caseID167

Double-Diaphragm Pump – Warren Rupp

View

For this design, a series of machined stainless steel air valve spacers were replaced with zinc die castings. Because of the spacer’s large flow areas, engineered plastics do not have the required strength to maintain shape and rigidity. Die cast ZA-8 was chosen for...
driving2_photo2_caseID170

Driving Gears

View

This is an excellent alternative to engineering plastics, aluminium or milled – sintered steel for the realization of driving gears for toothed belts (electronics) or pinion engagement (building, mechanical, precision hardware). Off-tool net shape thin wall zinc die...
ezifill2_photo2_caseID173

Ezi – Fill Fuel Dispenser

View

Its strength, tolerance for accurate detailing, non-corrosive properties compared to aluminium, and production speeds (faster than plastic) made die cast zinc the obvious solution when it came to the manufacture of Unicast’s “Ezi – Fill” fuel dispenser. Manufactured...
4a2_photo2_caseID135

Foot Switch – Control International

View

Over time, the costs associated with machining the cast-iron switch cover eroded manufacturing margins. The decision was then made to zinc die cast the cover. Zinc had the density and weight Control International specified, and it provided better fit, quality, and...
frameco2_photo2_caseID113

Frame Cover

View

The high dimensional tolerances possible with zinc die casting permitted precise and reliable seating of 6 bushings, diameter 8 mm/0.31 inches, with a diametral tolerance of ± 0.015 mm without additional machining. The complex shapes achievable in zinc die casting...
gridmod2_photo2_caseID116

Grid Module

View

Mosaic mimic panels form a display system that provides an overall picture of complex operations and gives technicians the ability to monitor and control events. The system’s main advantage is its modular design, providing flexibility for easy modification and...
housinb2_photo2_caseID90

Housing and Base Plate

View

Originally, the housing and base plate frame were sand cast aluminium and finish machined. Machining and assembly time took 3.5 hours per unit. During a redesign, the company set about to reduce costs without sacrificing quality or performance. This led to graphite...

Housing for low voltage angle gear drive

View

This casting is a segment of a multi-piece gearbox for 24/48 volt engines. The cost pressure in the market segment prompted the designers to rethink. A cost-effective production method for manufacturing the individual components that does not require any further...

Housing MX bottom shell R2S3

View

With this modular concept, various pluggable, cast housing components can be installed in the system as required. The concept implements a new, complex and resource-saving control cabinet technology. The combination of system function modules and a housing base...
housinp2_photo2_caseID92

Housing, Plate, and Anvil

View

Complexity of the shapes allows for the integration of multiple positions. The non-magnetic character of the zinc alloys compared to the plastics work in favor of the design’s long term dimensional stability and reliability.
linkalu2_photo2_caseID100

Link Between Aluminium Structural Beam

View

The aluminium structural beam must strongly fostered with water proofing to avoid penetration from the rain or washing water. The geometric position must be sound, and operating live must be assured.
modular2_photo2_caseID179

Modular Base Plate

View

This part is a modular base plate working in a pneumatic environment. Its function is to transport air between an air distributor and a jack. Modular base plates are made of pressure die cast Zamak 5 (ZA4UIG). The excellent fluidity of zinc alloys provides a surface...

MX housing bottom shell

View

A product extension has been developed for an innovative modular control cabinet solution from Beckhoff, based on the plug-and-play principle. A cast base shell has been designed for a new module that can be plugged into the modular system. Since control cabinets and...
paperfe2_photo2_caseID109

Paper Feeding Guide for Thermic Printer

View

The anti-magnetic character of the zinc alloys combined with the economic advantages of the production process win over the press formed steel sheet and aluminium profiles.
quickclamp2_photo2_caseID182

Quickclamp Air Prep System – IMI Norgren

View

A newly designed air preparation system utilizes zinc die casting for the major components of the Quickclamp(TM) assembly (as well as the bodies, bowls, and accessory parts of the filters, regulators and lubricators). Die cast zinc provides greater strength than...
reducto2_photo2_caseID147

Reductor

View

Zinc’s excellent bearing properties at high loads and low speeds permitted it to be used for this part without the use of pressed-in bronze bearings, reducing cost. The required dimensional precision and high required strengths also made zinc die casting the preferred...
roofbol2_photo2_caseID148

Roof-Bolt Wedge Anchors

View

When the AKZO Salt Company had problems getting roof-bolt wedge anchors from its malleable-iron foundry supplier, it opened the door for zinc alloy. Mine management set out to find an alternative source for these vital parts, but they were unable to find another...

Shielded connector for electrical engineering

View

Plug connections in electrical engineering are highly complex components that have to be delicate yet stable due to the space available. Added to this is the shielding function of different conductors in the housing. The award-winning shield housing is a true...
strapad2_photo2_caseID186

Strap Adapter, Entry Slide Mount, Belt Sheave

View

Die casting the three components in ZA-27 alloy offers attractive aesthetics and a near-net shape, which eliminates machining costs. In addition, ZA-27 alloy provides good wear and bearing characteristics.
topandb2_photo2_caseID155

Top and bottom sensor plate – dollar bill changer

View

A dollar bill changer incorporated top and bottom sensor plates fabricated from welded stamped components. The weldments could not hold tolerances greater than +/- 0.020 in. In an effort to resolve dimensional instability and fit problems, the manufacturer, working...
tunerho2_photo2_caseID157

Tuner Housing

View

Two M4 threads were needed on this zinc die casting in Z410 alloy (equivalent to BS 1004B). Because the holes were at 90° and in different planes, the threading could not be carried out in a single operation. By comparison with two separate threading operations, it...