The casting design was engineered to provide the surface finish on the decorative areas while providing adequate strength and reducing cost. The existing weldment design was problematic because of the metal fill direction through the cavity. Working with the customer,...
Modern printers require a pin support which must be cast pore free, non-deformable, and of precise dimensions. Because of the large numbers of units produced, the life of the die is a determining factor. From the client’s point of view, the sound dampening qualities...
As an individual part, the award-winning casting is a very filigree, long and sensitive component. Four individual and very thin conductor strands with dimensions in the millimeter range have to be produced by casting with a cross-section of perhaps just one...
This part was cast with Zincopor(R) technology, which resulted in a weight reduction of 25%. With an annual production rate of 235,000 part/year, this represents a 10-ton reduction of zinc alloy.
Micro-informatics are already an integral part of business and professional life. The will soon be present everywhere, including the home. What role do zinc alloys play? This back cover for a microcomputer illustrates how zinc die castings can simplify design and...
Key material requirements for the office bundling machine are hardness and strength, the ability to hold good tolerances, and lubricity. ZA-27 was selected as the die casting material because of its hardness, strength, dimensional stability, and natural lubricity. By...
Handle recesses and push-button covers for electronic front door locks and windows increasingly have to fulfill more than just mechanical functions; they are now being equipped with electronics to enable fingerprint access, integrate LED lighting, and control electric...
Third Place, 2018 EU Zinc Die Casting Competition This component in the field of office technology is a successful example of composite casting. In this case, zinc is cast with inserts made of stainless steel in order to optimally exploit the properties of both...
The part is machined on guiding bores and reference faces. It substitutes for the pressed steel plate for several reasons: its high precision realized on machined diameters Ø < 0.02 mm and for the cost efficiency.
Zinc alloy pressure die casting has been chosen by the IER company for the four parts that make up the structure of this ticket printer. The specification set by IER required materials and technology that would enable the production of: complex shapes, so that the...
The SUDHAUS key safe is a secure storage place for keys and other valuables. The dimensions were chosen so that bunches of keys and credit card formats can be stored. Areas of application include contactless key handover for holiday homes, rental car collection/return...
Océ Graphics – one of the world’s leading manufacturers of tracing machines – uses zinc alloy die castings in each of the seven machines in its range. Zinc alloy castings form part of the structure of the machines, through the two side plates and two grips in the...
The platen housing design incorporates three previous parts. In order to function properly, the material must be rigid and strong. The housing is cast with four elongated slots, four deep slots, and seven cored holes, maximizing the need for structural support. In...