Casting Techniques: Pressure Die Casting

panelnu2_photo2_caseID108

Panel Nut – Ignition Switch

View

Ignition switch corrosion was the source of customer frustration and concern. Standard panel nuts, like the ones used to secure the ignition switch to the riding mower control panel, are made of stamped steel. The die cast company’s technical staff proposed changing...
motorch2_photo2_caseID118

Motor Chassis

View

This chassis for a motor drive unit for an automatic opening roller door was made from several pressed metal parts prior to being designed as a zinc die casting. Die casting in zinc alloy 3 provided numerous benefits: 1.) Additional features such as pockets, the...
modular2_photo2_caseID179

Modular Base Plate

View

This part is a modular base plate working in a pneumatic environment. Its function is to transport air between an air distributor and a jack. Modular base plates are made of pressure die cast Zamak 5 (ZA4UIG). The excellent fluidity of zinc alloys provides a surface...

Mobile Radio Antenna

View

Zinc die casting was chosen to reduce cost of an antenna base for mobile radio equipment, which was originally a brass screw-machined part. Powder metallurgy was evaluated, but it couldn’t achieve the required undercuts without machining. Zamak 2 alloy was specified...
gearbox2_photo2_caseID129

Miter Gear Box – Hunter Douglas Venetian Blind

View

A four-piece miter gear assembly utilized zinc die casting for strength and precision. Both pinion gear shafts and housing halves are die cast net-shape, achieving full functionality without a cost penalty compared to alternative designs (thermoplastic housing/gears...