Housing for KitchenAid Coffee Machine

View

The 9,5 kg zamak housing of this designer coffee machine is made from 8 zinc pressure die cast parts with weights between 2.2 kg and 75 g. The parts are powder coated. To avoid any bubbles during thermal curing of the paint, the parts are vacuum cast to avoid gas...
ima01

Automotive Shift Level

View

This shift lever connects the shifter and the gear in ZF automotive gearboxes. This part was originally cast in aluminum but required tapping and other secondary operations in order to meet the close tolerances. Thanks to close collaboration with the customer, the...
ima15

Connector for Radio AM/FM Signal

View

The part has the following attributes: One of this part’s highlights is its functionality—it allows one single part in Zamak for electrical connection (interface) and mechanical (coding + retention). It also has a connector function, which allows for the transmission...
ima14

Electronic Connector

View

The key benefits to this product’s design was a close cooperation between die caster and customer through a clipping system. It utilizes modern assembling technology, and because it does not involve a screw, creep is not a risk.
ima13

Dental – Occlusal Bite Holder Block

View

The medical sector is a highly demanding, niche market. The main benefit of using zinc die casting for this product is the outstanding surface quality achieved.