The part is machined on guiding bores and reference faces. It substitutes for the pressed steel plate for several reasons: its high precision realized on machined diameters Ø < 0.02 mm and for the cost efficiency.  

Planter Handler

View

The planter handle is used to adjust spring force to a pair of closing wheels. It is important for the handle to be durable, easily accessible, and very comfortable to grip. To accent product appearance, designers chose a die cast over a welded fabrication. Die cast...
perfume2_photo2_caseID111

Perfume Vaporizer for Hand Bags

View

This set of six parts, four of which are made of Zamak, makes up a rechargeable perfume vaporizer. There are several notable characteristics of the final product that illustrate the versatility of the zinc alloy pressure die casting process: complexity of the assembly...
hub2_photo2_caseID110 (1)

Peerless Pull-Out Faucet – Delta

View

Initially, the hub–two intersecting cylinders–was a brazed assembly. Cylinders were screw machined from solid brass. Operations included turning, drilling, internal milling, cut-off, and rolling of one cylinder end to accept a plastic transition piece. The redesigned...
paperfe2_photo2_caseID109

Paper Feeding Guide for Thermic Printer

View

The anti-magnetic character of the zinc alloys combined with the economic advantages of the production process win over the press formed steel sheet and aluminium profiles.