Casting Techniques: Gravity Casting

visecom2_photo2_caseID160

Vise Components

View

Eight separate ZA-12 alloy castings are utilized in the TUCKER woodworking vise. Castings form the pivot block, front jaw, rear jaw, quick-release nut, yoke, stanchion, mounting plate, and keeper plate. Based on the shapes needed to form the vise, casting easily...
trimfra2_photo2_caseID156

Trim Frame

View

The instrument incorporates two frames, one for the front panel and another in the rear. Originally the frames were designed as welded aluminium extrusions. In search of alternative methods, the manufacturer looked to zinc graphite permanent mould casting with its low...
housinb2_photo2_caseID90

Housing and Base Plate

View

Originally, the housing and base plate frame were sand cast aluminium and finish machined. Machining and assembly time took 3.5 hours per unit. During a redesign, the company set about to reduce costs without sacrificing quality or performance. This led to graphite...
electri2_photo2_caseID133

Electrical Auxiliary Switch Cam

View

A starter for large horse-power motors incorporated a fabricated sheet-metal cam bolted to a bracket and welded to a shaft. To simplify manufacturing and reduce cost, the cam design was changed to a single-piece ZA-12, graphite permanent mold casting. Additionally,...
drivede2_photo2_caseID132

Drive Beck

View

The drive deck for Cherokee’s 5-1/4 in. WORM optical drive utilizes a ZA-12 graphite permanent mold casting. From the start, graphite permanent mold was the process of choice because of its economical tooling cost, good dimensional control, and low-volume economies....