Application Fields: Electrical/Electronics
View
This casting is a segment of a multi-piece gearbox for 24/48 volt engines. The cost pressure in the market segment prompted the designers to rethink. A cost-effective production method for manufacturing the individual components that does not require any further...
View
As an individual part, the award-winning casting is a very filigree, long and sensitive component. Four individual and very thin conductor strands with dimensions in the millimeter range have to be produced by casting with a cross-section of perhaps just one...
View
First Place, 2018 EU Zinc Die Casting Competition The housing is cast with extremely thin walls of up to 0.5 millimeters – in the cast thread with an incline of even up to 0.2 millimeters – wall thickness and thus places the highest demands on toolmaking...
View
Gold Award Winner from China Best Diecasting 2018 This part was an existing part already but brass has been substituted by Zamak5 alloy. It is thin wall, min 0.5mm, and electroplated, so it has high surface requirements for surface roughness, cold shuts, and...
View
Together, these two parts form a protective casing for the internal components of traffic lights. The material properties provide protection against vandalism and have much longer lifetimes than polymer materials. Due to thinner sections, they are also lighter than...
Page 2 of 6«12345...»Last »