Major Selection Criteria: High Mass

Control Handles and Mounting Box

View

ZA-12 graphite permanent mold castings are used for the gunner’s control handles and mounting box because the process is an economical low-volume casting method. ZA-12 also provides the handles with the density to simulate steel. Graphite permanent mold casting is...