The zinc pressure die cast corner stake, fastened with pop rivets, fits tightly into the Galvabond roll form section of the door. It has to compete with plastic molded, aluminium extruded, and aluminium pressed parts’ this is because of the many properties of the zinc...
View
This range of pens – the “Golf” series – is characterized by clean lines and an antique appearance produced by symbols in fine relief on the surface. The thin castings – wall thickness of 0.7 mm – have enabled the total weight to be kept low, while the technology of...
View
The Delta Faucet’s construction is known as shell technology. It features a die-cast zinc cover, or escutcheon, over a brazed copper and brass assembly. The thin zinc cover is much more uniform than brass; it provides near net shape die casting with tolerances of...