Alloys: ZA-12 (ZA12, ZL1110, ZnAI11Cu1)
View
ZA-12 graphite permanent mold castings are used for the gunner’s control handles and mounting box because the process is an economical low-volume casting method. ZA-12 also provides the handles with the density to simulate steel. Graphite permanent mold casting is...