Alloys: ACuZinc5 (Acuzinc5, ZL0350, ZnAI3Cu5)
View
One of the first opportunities to test ACuZinc 5 was in Delphi Interior and Lighting System’s newly-designed heliscrew horizontal actuator for power seats. The die castings replace a powder-metal gear rack and plastic gear housing design. Seat adjustment is comparable...