In their original version, these parts were produced in glass fiber reinforced resin, 3-4.5 mm thick and containing two brass inserts to fix them to the car body. These components are painted on the body to match the rest of the car. Problems encountered during...
This shift lever connects the shifter and the gear in ZF automotive gearboxes. This part was originally cast in aluminum but required tapping and other secondary operations in order to meet the close tolerances. Thanks to close collaboration with the customer, the...
Excellence Award Winner from China Best Diecasting 2018 This part has a high level of fine detail and an excellent surface finish after plating. It is difficult to cast and ejection needs to be done carefully to avoid any deformation. The casting process is very...
Utilizing zinc alloys to create this part allowed for outstanding control of each step and parameter involved in the full process, from design to final part to achieve, to achieve the perfect design. With die casting, the same surface quality and appearance could be...
The lever was originally designed as a steel sand casting with machining operations to size the shaft, pivot hubs, and cable connection holes. The final operation was a zinc plating. After a value analysis of an all-metal foot pedal control system, the materials...
Engineers decreased time-to-market by utilizing existing gear housing tooling to develop a higher load winch. Superwinch’s 1,500-lb. unit incorporated two 380 Aluminium die cast housings which functioned as rotating and stationary ring gears. By substituting ZA-27...
This casting part was originally produced in die cast aluminum. It could be produced only with disproportionate effort and high scrap rates. The parting plane in the casting could never reach the surface quality standards because at that position was a vacuum...
One of the first opportunities to test ACuZinc 5 was in Delphi Interior and Lighting System’s newly-designed heliscrew horizontal actuator for power seats. The die castings replace a powder-metal gear rack and plastic gear housing design. Seat adjustment is comparable...
Due to its reliability, zinc allows the mounting of a precision bearing of an air turbine with a bevel gear. It also allows the plastic over coating. Zinc fulfilled the requirements for this design, including strength with precise shapes and thread with repetition at...
Warner Gear’s 4WD locking hub takes advantage of ZA-8’s net shape castability, creep resistance, and excellent finishing characteristics to provide a highly functional and aesthetic cover. ZA-8 alloy was chosen because it handles temperatures close to 200 degrees F, a...
The rigidity of this part ensures the quality of retro-vision due to the absorption of the vibrations compared to engineering plastics. Note the (omega) shape for the rigidity of the assembly. Rigidity inside the envelope (volume) and reduced width of the assembly...
This chassis for a motor drive unit for an automatic opening roller door was made from several pressed metal parts prior to being designed as a zinc die casting. Die casting in zinc alloy 3 provided numerous benefits: 1.) Additional features such as pockets, the...
The seats in luxury cars are moved forwards and backwards by motorized reduction gears which must be solid, reliable, accurate, and mechanically strong. Zinc alloys satisfy these requirements and offer the added benefit of noise reduction due to their density.
People carry this cast part with them in many variations: a design element of the car key. The demand for a high-quality look, an appealing, cool feel and the requirements for a robust, largely scratch-resistant surface led to the decision to use zinc as a material....
The award-winning cast part in the automotive category is a basic lever for the shift lever of an automatic transmission in a car. The gearshift knob is in the constant field of vision of the driver and the vehicle occupants, which places very high demands on the...
Key benefits include: Design and use of a complex tool to avoid multiple secondary operation. Excellent gating control to achieve mechanical tolerances.
The original selector tube was designed as a magnesium-steel assembly. It was redesigned as a one-piece ZA-8 alloy die casting. The ZA-8 casting replaced steel without loss of torque strength. Net shape casting produces a complex, multifunctional component. The...