Feedhorn incorporates six graphite permanent mold castings, including the end cap, housing (which holds the circuit boards), feedhorn, cover (used for shielding), and two mounting probes. ZA-12 alloy provides the components with the necessary strength to withstand the...
The casting design was engineered to provide the surface finish on the decorative areas while providing adequate strength and reducing cost. The existing weldment design was problematic because of the metal fill direction through the cavity. Working with the customer,...
As an individual part, the award-winning casting is a very filigree, long and sensitive component. Four individual and very thin conductor strands with dimensions in the millimeter range have to be produced by casting with a cross-section of perhaps just one...
ZA-12 graphite permanent mold castings are used for the gunner’s control handles and mounting box because the process is an economical low-volume casting method. ZA-12 also provides the handles with the density to simulate steel. Graphite permanent mold casting is...
Over time, the costs associated with machining the cast-iron switch cover eroded manufacturing margins. The decision was then made to zinc die cast the cover. Zinc had the density and weight Control International specified, and it provided better fit, quality, and...
Engineers decreased time-to-market by utilizing existing gear housing tooling to develop a higher load winch. Superwinch’s 1,500-lb. unit incorporated two 380 Aluminium die cast housings which functioned as rotating and stationary ring gears. By substituting ZA-27...
Operating at pressures ranging from 50 to 125 psi, the Danair Aerosmith hammer delivers up to 1,000 hammer blows per minute. During the early production phase finish machining exposed casting porosity and the cast iron air grille vents frequently broke during service....
This zinc alloy part is designed to raise the global quality perception of the final product. The dimensional precision of the process for the fine fitting of different sub assemblies and the long life of the mold and tooling for large production series led the choice...
The elements of this equipment (TYCAS) were created to detect the positions of approaching aircraft according to new security norms of the IATA. The process proved to be more economical compared to traditional machining despite limited series and to pressure die cast...
Originally, the housing and base plate frame were sand cast aluminium and finish machined. Machining and assembly time took 3.5 hours per unit. During a redesign, the company set about to reduce costs without sacrificing quality or performance. This led to graphite...
This product has been created for a top quality, guaranteed-for-life hacksaw. Zinc alloys satisfy the surface coating and the mechanical resistance required for the handle and saw blade guide, with the process economy for a high-quality product on a competitive...
The planter handle is used to adjust spring force to a pair of closing wheels. It is important for the handle to be durable, easily accessible, and very comfortable to grip. To accent product appearance, designers chose a die cast over a welded fabrication. Die cast...
The goal of product designers for the 1/4 in. air ratchet was to lower product manufacturing costs while improving performance and appearance. The original product design specified an axial assembly–a machined steel head attached by a lock nut to a housing handle....
A zinc die-casting application in the absolute premium range: This award-winning cast part is tangible on the steering wheel of a Porsche sports car and makes acceleration an experience. The paddles are attached to both sides of the back of the steering wheel and are...
The SUDHAUS key safe is a secure storage place for keys and other valuables. The dimensions were chosen so that bunches of keys and credit card formats can be stored. Areas of application include contactless key handover for holiday homes, rental car collection/return...
The instrument incorporates two frames, one for the front panel and another in the rear. Originally the frames were designed as welded aluminium extrusions. In search of alternative methods, the manufacturer looked to zinc graphite permanent mould casting with its low...
When Black & Decker decided to introduce a new manual staple gun, designers and engineers started with a clean slate. Their goal was to integrate efficiency, simplicity, and ergonomics into the new tool. The result is a radical design that moves the handle pivot...
Eight separate ZA-12 alloy castings are utilized in the TUCKER woodworking vise. Castings form the pivot block, front jaw, rear jaw, quick-release nut, yoke, stanchion, mounting plate, and keeper plate. Based on the shapes needed to form the vise, casting easily...