Casting Study: Thermostate Valve Housing
Special features of this die cast product include precise dimensions that ensure a perfect fit around the circumference of the housing, making it water-resistant so that the internal components are protected. The tool design allows for uniform filling and casting with a fast cycle time. A range of wall thickness differences are required to meet structural requirements, this required special processing to achieve high quality surface finish and tight tolerances.
Weight of the part: 1180g
Total casting weight: 2640g
Dimension: 300 x 130x 68mm