Casting Study: Inking Stamp for Post Office Franking Machine

Major Selection Criteria: Good Finish, Mechanical Properties, Net Shape
Alloy: Zamak 5 (ZL5, ZL0410, ZnAI4Cu1, alloy 5)
Application Field: Business/Office Equipment
Application Size: 30 x 25 mm
Surface Finish: As-Cast
Casting Technique: Pressure Die Casting
Source: NEOPOST

inkings2_photo2_caseID94This design is an interchangeable stamp on a franking machine. It is coated with ink on the summit of the engraving and stamps the envelope.