antenna LNB die casting

Antenna LNB/Feedhorn Assembly

View

Feedhorn incorporates six graphite permanent mold castings, including the end cap, housing (which holds the circuit boards), feedhorn, cover (used for shielding), and two mounting probes. ZA-12 alloy provides the components with the necessary strength to withstand the...

Control Handles and Mounting Box

View

ZA-12 graphite permanent mold castings are used for the gunner’s control handles and mounting box because the process is an economical low-volume casting method. ZA-12 also provides the handles with the density to simulate steel. Graphite permanent mold casting is...
drivede2_photo2_caseID132

Drive Beck

View

The drive deck for Cherokee’s 5-1/4 in. WORM optical drive utilizes a ZA-12 graphite permanent mold casting. From the start, graphite permanent mold was the process of choice because of its economical tooling cost, good dimensional control, and low-volume economies....
electri2_photo2_caseID133

Electrical Auxiliary Switch Cam

View

A starter for large horse-power motors incorporated a fabricated sheet-metal cam bolted to a bracket and welded to a shaft. To simplify manufacturing and reduce cost, the cam design was changed to a single-piece ZA-12, graphite permanent mold casting. Additionally,...
hammerc2_photo2_caseID81

Hammer Cap

View

Operating at pressures ranging from 50 to 125 psi, the Danair Aerosmith hammer delivers up to 1,000 hammer blows per minute. During the early production phase finish machining exposed casting porosity and the cast iron air grille vents frequently broke during service....
housinb2_photo2_caseID90

Housing and Base Plate

View

Originally, the housing and base plate frame were sand cast aluminium and finish machined. Machining and assembly time took 3.5 hours per unit. During a redesign, the company set about to reduce costs without sacrificing quality or performance. This led to graphite...
lowspee2_photo2_caseID103

Low-Speed, High-Load Bearings

View

The Champion Series IV grader incorporates ZA-12 alloy low-speed, high load bearing to improve operation performance. This Front Axle Bearing application acts as a replacement for the grader’s front axle needle bearings. The original needle bearings performed well...

Planter Handler

View

The planter handle is used to adjust spring force to a pair of closing wheels. It is important for the handle to be durable, easily accessible, and very comfortable to grip. To accent product appearance, designers chose a die cast over a welded fabrication. Die cast...
roofbol2_photo2_caseID148

Roof-Bolt Wedge Anchors

View

When the AKZO Salt Company had problems getting roof-bolt wedge anchors from its malleable-iron foundry supplier, it opened the door for zinc alloy. Mine management set out to find an alternative source for these vital parts, but they were unable to find another...
trimfra2_photo2_caseID156

Trim Frame

View

The instrument incorporates two frames, one for the front panel and another in the rear. Originally the frames were designed as welded aluminium extrusions. In search of alternative methods, the manufacturer looked to zinc graphite permanent mould casting with its low...
visecom2_photo2_caseID160

Vise Components

View

Eight separate ZA-12 alloy castings are utilized in the TUCKER woodworking vise. Castings form the pivot block, front jaw, rear jaw, quick-release nut, yoke, stanchion, mounting plate, and keeper plate. Based on the shapes needed to form the vise, casting easily...